Add to Cart
Quick Detail:
Description:
The cnc carbide lathe insert is made of innovative cemented carbide raw materials commonly used for steel and stainless steel, so that the blade has excellent performance of high toughness, high wear resistance and high temperature resistance; Unique coating process, fine and smooth, no drip marks, reduce surface friction, so that the cutting resistance is smaller; Carbide with special crystal structure is processed by German technology, which makes the blade have high hardness, good toughness and high temperature resistance. The overall hardness is stronger, and the cutting edge is more sharp and wear-resistant; Sharp cutting, 3 corners available, easy and labor-saving; Reduce cutting resistance to achieve sharp cutting; Various groove types and complete specifications meet your various processing needs from different angles.
Specifications:
Brand | BWIN |
Model | 16ER/16IR 18UN |
Color | Black/Yellow |
Workpiece | Stainless steel/Cast iron/Steel |
Type | Metal CNC Carbide Lathe Cutting Tool |
Material | Carbide Threading Cutting Insert |
Processing Type | Medium Cutting |
Feature | High strength |
High durability | |
Sharp and durable | |
Smooth chip breaking | |
Fine cutting | |
Standard | ISO |
Quantity | 10pcs/box |
Weight | 0.015kg |
Package | Plastic Box |
Customized Support | OEM, ODM |
Lead Time:
antity(pieces) | 1 - 3000 | >3000 |
Lead time (days) | 7 | To be negotiated |
Notice:
Thread turning is characterized by large cutting resistance, easy tool vibration, difficult chip removal, difficult cooling, and complex programming. Therefore, the following matters should be paid attention to during processing:
Applications:
Our carbide lathe insert could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:
Advantages:
1. Honest merchants, reasonable price and quality assurance
2. Large inventory, sufficient supply and high cost performance
3. Customer service responds in time and delivers goods quickly
4. Provide after-sale guarantee to make your after-sale service free
1. Rear cutter face wear: (This is a common practical form)
Influence: the workpiece size gradually changes or the surface light intensity decreases
Cause: The linear speed is too high, reaching the service life of the tool
Measures: Adjust the processing parameters, such as reducing the linear speed and using a blade with higher wear resistance
2. Blade breakage: (bad actual effect form)
Effect: sudden change of workpiece size or surface smoothness, resulting in burrs on the spark surface
Cause: Improper parameter setting, improper tool face material selection, poor workpiece rigidity, unstable blade clamping Measures: check whether the parameter setting is reasonable, and select the corresponding tool according to the workpiece material
3. Serious fracture: (very bad actual effect form)
Effect: sudden and unexpected occurrence, resulting in scrapping of tool handle materials or defective and scrapped workpieces
Cause: The processing parameters are set incorrectly, and the vibrating tool workpiece or blade is not installed in place
Measures: set reasonable parameters, reduce the feed rate and chip, select the corresponding processing blade, and strengthen the rigidity of the workpiece and blade
4. Chips:
Effect: the size of the workpiece is inconsistent, the surface finish is poor, and the workpiece surface is attached with fluff or burrs. Cause: the cutting speed is too low, the feed is too low, and the blade is not sharp enough
Measures: improve the cutting speed, and use blades with higher sharpness for feed rate